Failure mechanism of aluminium – carbon fibre reinforced polymer interlocking joints through punching
Eurecat, Centre Tecnològic de Catalunya, Unit of Polymeric and Composite Processes, Av. Universitat Autònoma 23, 08290, Cerdanyola del Vallès, Spain; AMADE, Polytechnic School, University of Girona, Av. Universitat de Girona, 4, 17003, Girona, Spain.
AMADE, Polytechnic School, University of Girona, Av. Universitat de Girona, 4, 17003, Girona, Spain.
Luleå University of Technology, Department of Engineering Sciences and Mathematics, Solid Mechanics. Eurecat, Centre Tecnològic de Catalunya, Unit of Polymeric and Composite Processes, Av. Universitat Autònoma 23, 08290, Cerdanyola del Vallès, Spain.ORCID iD: 0000-0003-4720-7888
AMADE, Polytechnic School, University of Girona, Av. Universitat de Girona, 4, 17003, Girona, Spain.
2025 (English)In: International Journal of Lightweight Materials and Manufacture, E-ISSN 2588-8404, Vol. 8, no 5, p. 611-622Article in journal (Refereed) Published
Abstract [en]

Single-Step Punch Interlocking (SSPI) is a recently developed joining methodology between aluminium and Carbon Fibre Reinforced Polymer (CFRP) aiming to contribute to multi-material design of structural parts. This hybrid joint technology combines adhesive bonding with mechanical interlocking. Elucidating the failure mechanism of the developed joint is relevant to provide insights for future enhancements in performance, increase its lifespan and prevent premature failure. Therefore, the different subcritical failure events were identified through interrupted Single-Lap Shear (SLS) tests and subsequent non-destructive ultrasonic inspection, and the global failure mechanism was described. Results indicate that the addition of the SSPI joint delayed the onset and propagation of adhesive failure between both substrates, providing residual strength and increasing the ultimate load in a 65 % and the absorbed energy of the joint in a 156 %.

Place, publisher, year, edition, pages
KeAi Publishing Communications Ltd. , 2025. Vol. 8, no 5, p. 611-622
Keywords [en]
Aluminium, CFRP, Joint, Failure mechanism, Ultrasound testing, Single-lap shear
National Category
Composite Science and Engineering
Research subject
Solid Mechanics
Identifiers
URN: urn:nbn:se:ltu:diva-114190DOI: 10.1016/j.ijlmm.2025.01.002ISI: 001554125700001Scopus ID: 2-s2.0-105010854014OAI: oai:DiVA.org:ltu-114190DiVA, id: diva2:1987361
Note

Validerad;2025;Nivå 1;2025-08-06 (u5);

Full text license: CC BY-NC-ND 4.0;

Funder: Catalan Government

Available from: 2025-08-06 Created: 2025-08-06 Last updated: 2025-11-28Bibliographically approved

Open Access in DiVA

fulltext(4103 kB)113 downloads
File information
File name FULLTEXT01.pdfFile size 4103 kBChecksum SHA-512
c193dd58ac89ea951e6ac0ec5acf51856496d75608931ab8a57284cc63eb2c68b85a90861f5838e14b45a1548fffe7e964bdc38bd43740611eadaa471284ac50
Type fulltextMimetype application/pdf

Other links

Publisher's full textScopus

Search in DiVA

By author/editor
Casellas, Daniel
By organisation
Solid Mechanics
Composite Science and Engineering

Search outside of DiVA

GoogleGoogle Scholar
Total: 115 downloads
The number of downloads is the sum of all downloads of full texts. It may include eg previous versions that are now no longer available

doi
urn-nbn

Altmetric score

doi
urn-nbn
Total: 845 hits
CiteExportLink to record
Permanent link

Direct link
Cite
Citation style
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Other style
More styles
Language
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Other locale
More languages
Output format
  • html
  • text
  • asciidoc
  • rtf