Effect of surface roughness and residual stress on high-cycle fatigue behaviour of PM-HIP duplex stainless steel
2025 (English)Independent thesis Advanced level (degree of Master (Two Years)), 20 credits / 30 HE credits
Student thesisAlternative title
Ytans beskaffenhet och restspänningars påverkan på högcykelutmattning hos PM-HIP duplex rostfritt stål (Swedish)
Abstract [en]
This thesis examines how surface structure and residual stresses in PM-HIP duplex stainless steel affect fatigue behaviour under cyclic loading. Test specimens were produced from powder material using hot isostatic pressing with high pressure and temperature. After pressing, the specimens were pickled, with half of them further processed so that one side remains the pickling while the others are fully machined. This resulted in two different surface conditions.To study the surface, profilometry was used to generate 2D, 3D surface topography maps along with surface roughness parameters. Results indicate that Sa values in machined samples were approximately 50 times lower than those of pickled samples. Similarly, Sz and Sq values follow this trend, indicating smoother machined surfaces. Additionally, Ssk measurements show that the machined specimens had both high positive and negative values, suggesting more peaks onthe surface, whereas the pickled surface had more valley-dominated surfaces, with irregularities resulting from the pickling process. These surface defects can create stress concentrations, increasing the risk of crack initiation within one of the many pits formed during the treatment.To assess internal stresses, X-ray diffraction scans was conducted. The analysis reveals that machined specimens show higher positive residual stresses, meaning they have TRS resulting from machining, which can reduce fatigue life and increase crack formation, typically near surface inclusions. Meanwhile, compressive residual stress, beneficial for fatigue resistance,was presented in both cases, though pickled samples display values closer to zero, indicating less residual stress. Finally, to evaluate mechanical strength, four-point bending tests were conducted to measure stress distribution. The results expose that machined specimens withstand higher loads before failure, meaning they have better fatigue strength and are more suitable for demanding environments. Specifically, the mean fatigue strength at 106 cycles is 315 ± 23 𝑀𝑃𝑎 formachined samples, whereas pickled specimens show a lower fatigue strength of 187,5 ±29,9 𝑀𝑃𝑎. In summary, surface roughness, residual stress, stress levels, and material defects affect fatigue performance. Machined surfaces offer high fatigue strength due to their smooth texture but require post-treatment to counter tensile residual stress. Pickled surfaces reduce residual stress but have greater roughness and defects, leading to lower fatigue strength. Optimizing surface treatment is essential for enhancing fatigue performance.
Place, publisher, year, edition, pages
2025.
Keywords [en]
Powder metallurgy, Hot isostatic pressing; Duplex stainless steel; surface roughness; residual stress; fatigue behaviour
National Category
Materials Engineering
Identifiers
URN: urn:nbn:se:kau:diva-106374OAI: oai:DiVA.org:kau-106374DiVA, id: diva2:1986252
Subject / course
Mechanical Engineering
Educational program
Engineering: Mechanical Engineering, spec. in Materials Engineering (300 ECTS credits)
Supervisors
Examiners
2025-08-042025-07-302026-02-12Bibliographically approved