Toward Corrosion-Resistant Titanium Coatings Deposited by Magnetron Sputtering on Aluminium
2025 (English)Independent thesis Advanced level (professional degree), 20 credits / 30 HE credits
Student thesis
Abstract [en]
Aluminium is an attractive material for bipolar plates in fuel cells because of its lightweight andcost-effective properties, particularly when compared to stainless steel, which is the most widelyused in bipolar plates today. Using aluminium for bipolar plates would therefore significantly reduce the weight and cost of fuel cells, paving the way for broader commercial adoption. However, the environment in a fuel cell is highly corrosive and aluminium cannot be used without a protective surface treatment. To prevent corrosion damage, one can therefore coat aluminium with a thin layer of titanium, utilizing titanium’s great corrosion resistance while retaining the low weight and cost of aluminium. Previous work revealed the presence of defects in the titanium layer that are detrimental to the films corrosion resistance. The objective of this project is to understand why these unknown defects occur and prevent their formation to create a defect-free titanium film. In this work, titanium was deposited on an aluminium substrate using physical vapour deposition (PVD) techniques. Specifically, High power impulse magnetron sputtering (HiPIMS),and direct current magnetron sputtering (DCMS) was used to produce a thin-film with good adhesion and high density. Samples were prepared with varying titanium thicknesses, interlayers, substrates, and deposition parameters, and then analysed to assess film quality, defect origins, and deposition integrity. The defect density was analysed and the defects were categorised into three types. This showed that by using a thin aluminium interlayer one could greatly reduce the defect density and size. Further analysis revealed that all three types of defects originate from contaminants on the surface of the aluminium substrate. By modifying the cleaning process, specifically by adding a deionised water cleaning, the contamination could be removed. This led to a complete removal of the defects. However, care needs to be taken in the cleaning step, as exposure todeionised water for an extended period showed corrosion-induced defects on the final titanium layer. By employing this cleaning method in combination with HiPIMS deposition, a defect-freetitanium film with high density and excellent adhesion was achieved, thereby facilitating thefurther development of aluminium-based bipolar plates and corrosion-resistant coatings
Place, publisher, year, edition, pages
2025. , p. 45
Series
UPTEC Q, ISSN 1401-5773 ; 25010
National Category
Surface- and Corrosion Engineering
Identifiers
URN: urn:nbn:se:uu:diva-562346OAI: oai:DiVA.org:uu-562346DiVA, id: diva2:1978371
Educational program
Master Programme in Materials Engineering
Presentation
2025-06-12, 101132/Ångström, Lägerhyddsvägen 1, Uppsala, 11:33 (English)
Supervisors
Examiners
2025-06-302025-06-272025-06-30Bibliographically approved