On the Mechanical Behavior of Granite Material With Particular Emphasis on the Influence From Pre-Existing Cracks and Defects
KTH, Skolan för teknikvetenskap (SCI), Hållfasthetslära (Inst.). Atlas Copco Rock Drills AB, SE-70225 Orebro, Sweden..ORCID-id: 0000-0002-8645-4892
Grenoble Alpes Univ, Lab 3SR, F-38041 Grenoble, France..
Atlas Copco Rock Drills AB, SE-70225 Orebro, Sweden..
KTH, Skolan för teknikvetenskap (SCI), Hållfasthetslära (Inst.).ORCID-id: 0000-0001-6232-8819
Visa övriga samt affilieringar
2018 (Engelska)Ingår i: Journal of Testing and Evaluation, ISSN 0090-3973, E-ISSN 1945-7553, Vol. 46, nr 1, s. 33-45Artikel i tidskrift (Refereegranskat) Published
Abstract [en]

In this investigation, experiments were carried out in order to determine the mechanical properties of Bohus granite considering the influence from pre-existing cracks and defects. The experimental investigation aimed at a complete material characterization, for the purpose of mechanical analyses using advanced constitutive models, based on a variety of tests. In doing so, direct tensile and compression tests were performed to evaluate the stiffness and strength; quasi-oedometric tests were carried out in order to obtain the deviatoric and volumetric behavior of the material at different levels of hydrostatic pressure (up to 860 MPa); three-point bend tests were performed to evaluate the quasi-static strength of the rock and its distribution. Weibull statistics was then employed to describe the strength distribution. The intact specimens indicated a rather low scatter in the mechanical properties such as Young's modulus and tensile strength. However, specimens with large initial defects behaved differently. The failure mechanism in these specimens was not as brittle as the intact ones. The crack was opened on the tensile surface of such specimens during the three-point bend test at an early stage during loading, as demonstrated by digital image correlation results.

Ort, förlag, år, upplaga, sidor
AMER SOC TESTING MATERIALS , 2018. Vol. 46, nr 1, s. 33-45
Nyckelord [en]
granite, constitutive characterization, pre-existing cracks, quasi-oedometric, three-point bending, digital image correlation (DIC)
Nationell ämneskategori
Annan materialteknik
Identifikatorer
URN: urn:nbn:se:kth:diva-225332DOI: 10.1520/JTE20160072ISI: 000425663000005Scopus ID: 2-s2.0-85033563714OAI: oai:DiVA.org:kth-225332DiVA, id: diva2:1194582
Anmärkning

QC 20180403

Tillgänglig från: 2018-04-03 Skapad: 2018-04-03 Senast uppdaterad: 2024-03-18Bibliografiskt granskad

Open Access i DiVA

Fulltext saknas i DiVA

Övriga länkar

Förlagets fulltextScopus

Sök vidare i DiVA

Av författaren/redaktören
Saadati, MahidiLarsson, Per-Lennart
Av organisationen
Hållfasthetslära (Inst.)
I samma tidskrift
Journal of Testing and Evaluation
Annan materialteknik

Sök vidare utanför DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetricpoäng

doi
urn-nbn
Totalt: 142 träffar
RefereraExporteraLänk till posten
Permanent länk

Direktlänk
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annat format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annat språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf