Materialspecifikationens inverkan på skärbarheten: Ett projekt på uppdrag av Volvo Construction Equipment Arvika
Karlstad University, Faculty of Health, Science and Technology (starting 2013).
2015 (Swedish)Independent thesis Basic level (professional degree), 15 credits / 22,5 HE creditsStudent thesis
Abstract [sv]

Rapporten handlar om ett projekt på uppdrag av Volvo Construction Equipment i Arvika och utförs i kursen examensarbete för högskoleingenjörer i maskinteknik. I Arvika tillverkas hjullastare och man har periodvis spånproblematik vid bearbetning av hjullastarens ram. Man misstänker att spånproblematiken är kopplat till materialet i plåtarna som ingår i ramen, eftersom de köps in mot en materialspecifikation med generösa toleranser vilket man tror ger variationer i skärbarheten. Projektet handlar om att undersöka Volvos materialspecifikations inverkan på skärbarheten, och avgränsades till två plåtar i framramens nedre midja på modellen L150. Materialet i dessa två plåtar är S275JR med tjocklek på 30-40 mm. Frågeställningarna  är hur mycket varierar materialet inom materialspecifikationen? Vad ger detta för påverkningar på skärprocessen? Är den inlevererade plåten inom tolerans idag? Åtgärder som testades tidigt i projektet var att justera skärdata samt byta ut skär med hjälp av Volvos bearbetningsteknik, vilket inte gav önskat resultat. Vidare undersöktes plåtarnas certifikat som innehåller information om smältans kemiska analys och plåtens hållfasthetsvärden. Gällande projektets plåtar tillverkades de i stålverken SSAB och Dansteel, och certifikaten analyserades med hjälp av personer med kunskap om skärverktyg och metallurgi på bearbetningsavdelningen vid Seco Tools. Resultatet blev att stålet från SSAB innehöll teoretiskt ofördelaktigt låg svavelhalt (ca en promille), medan plåtarna från Dansteel hade stor variation på brottförlängningen som kan vara negativt för spånformningen. Bristande kommunikation mellan inköpsavdelningen och bearbetningsavdelningen upptäcktes, då informationen angående byte av plåtar inte når hela tillverkningskedjan. Kommunikationsbristen påverkade skärprocessen negativt. Åtgärder, rekommendationer och nya frågor har dykt upp med detta projekt. Slutligen har Volvo i samarbete med Seco Tools bearbetningslabb utfört tester med fyra olika Seco Tools skär i låg svavelhaltigt stål. Det prövades även varierande matning som en åtgärd för robust skärprocess. En rekommendation är att testa vidare för att undersöka om de teoretiska antagandena stämmer, och undersöka flera faktorer som spelar in för skärbarhet.

Abstract [en]

The report is about a project on behalf of Volvo Construction Equipment in Arvika and is included in the course thesis for graduate engineers in mechanical engineering. At Arvika factory, wheel loaders are manufactured and have periodically chip breaking problems in the cutting process of the wheel loader frame. It is suspected that the chip problems are linked to the materials in the plates because the structural steel is purchased against a material specification with generous tolerances, which they believe gives the variation in machinability. The project will involve investigating Volvo materials specification effect on machinability, and have narrowed to two plates in the front frame lower waist of the model L150. The material of these two plates is S275JR with thickness of 30-40 mm. The questions are how much varies the material in the material specification? What brings this to influences of the cutting process? What is the current situation, are the right plates delivered? Measures were proved early in the project, like adjust the cutting data and change cutting tools to another supplier, with the help of Volvo's processing technology. The changes did not give the desired results. The certificates of the plates were analyzed, containing information about the melt chemical analysis and the sheet strength values. The project's plates were manufactured in the steelworks SSAB and Dansteel, and the certificates were analyzed with the help of people with experience in tool cutting, metallurgy and processing of Seco Tools. The result was that the steel from SSAB contained theoretically too low sulfur content for contain good machinability, while plates from Dansteel had too big variety of elongation that may be negative for chip formation. Lack of communication between the purchase and processing department were discovered, because the information about change of plates does not reach the entire manufacturing chain, which affects the cutting process negatively. Actions, recommendations and new issues have shown with this project. Finally, Volvo in collaboration with Seco Tools processing lab performed tests with four different Seco Tools cuttings inserts in low- sulfur steel. It was also tested varying feed is as a good method for robust cutting process. One recommendation is to further investigate if the theory is correct, and test more factors which are important for machinability.

Place, publisher, year, edition, pages
2015. , 62 p.
Keyword [sv]
Spånbrytning, Konstruktionsstål
National Category
Natural Sciences
Identifiers
URN: urn:nbn:se:kau:diva-37653OAI: oai:DiVA.org:kau-37653DiVA: diva2:848202
Subject / course
Mechanical Engineering
Educational program
Study Programme in Mechanical Engineering
Presentation
2015-06-02, 21A342 Eva Ericsson, Karlstads Universitet, Karlstad, 12:37 (Swedish)
Supervisors
Examiners
Available from: 2015-09-04 Created: 2015-08-24 Last updated: 2015-09-04Bibliographically approved

Open Access in DiVA

Materialspecifikationens inverkan på skärbarhet(4754 kB)294 downloads
File information
File name FULLTEXT01.pdfFile size 4754 kBChecksum SHA-512
08d5252b75ee9f3bdb22e9e65c00848e78c810529719b2458d2c60811ef33e5ba4c83538ff2a18b43e4f6bed92917bd3293e5a26cf4e6a58344eb39cf966ddca
Type fulltextMimetype application/pdf

By organisation
Faculty of Health, Science and Technology (starting 2013)
Natural Sciences

Search outside of DiVA

GoogleGoogle Scholar
Total: 294 downloads
The number of downloads is the sum of all downloads of full texts. It may include eg previous versions that are now no longer available

urn-nbn

Altmetric score

urn-nbn
Total: 108 hits
CiteExportLink to record
Permanent link

Direct link
Cite
Citation style
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Other style
More styles
Language
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Other locale
More languages
Output format
  • html
  • text
  • asciidoc
  • rtf